目标分子:蛋白,多肽;基质:刚性,高度交联琼脂糖;平均粒径(Dv50):90-110 µm;功能基团:Sulfonate(-SO3-);离子载量:0.18 - 0.25 mmol H+/ml resin ;动态结合在两(DBC): >100 mg BSA/ ml resin(Dynamic binding capacity determined at 4-minutes residence time in the presence of 20 mM Na-citrate, pH 4.0);压力流速参数:2 bar at 900 cm/h(25 mm diameter column, 20 cm bed height);化学稳定性:与用于蛋白质纯化的所有标准水性缓冲液,1 M NaOH,30%异丙醇或70%乙醇兼容,不应在